ASTM A476-90(1997)
- Standard Specification for Ductile Iron Castings for Paper Mill Dryer Rolls (Withdrawn 2000)
- standard by ASTM International, 04/10/1997
- Publisher: ASTM
$23.00$46.80
1.1 This specification covers ductile iron castings for use in pressure containing paper mill dryer rolls at temperatures up to 450°F.
1.2 No precise quantitative relationship can be stated between the properties of the iron in various locations of the same casting or between the properties of a casting and those of a test specimen cast from the same iron (see Appendix X1).
1.3 A complete metric companion to Specification
Related Products
ASTM D7722-13
Standard Terminology Relating to Industrial Textile Stitches and Seams..
$20.00 $39.00
ASTM E23-12b
Standard Test Methods for Notched Bar Impact Testing of Metallic Materials ..
$38.00 $76.80
ASTM D5197-03
Standard Test Method for Determination of Formaldehyde and Other Carbonyl Compounds in Air (Active S..
$30.00 $60.00
ASTM D129-13
Standard Test Method for Sulfur in Petroleum Products (General High Pressure Decomposition Device..
$22.00 $44.00