• ASTM A608/A608M-12
Provide PDF Format

Learn More

ASTM A608/A608M-12

  • Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures
  • standard by ASTM International, 09/01/2012
  • Publisher: ASTM

$26.00$52.80


This specification covers the standard for iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures. The tubing shall be supplied in the as cast condition or as cast with machining on the outside or inside surfaces. The material shall conform to the required chemical composition in carbon, manganese, silicon, chromium, nickel, phosphorus, sulfur, and molybdenum. Tension test shall be performed in the tubing at elevated temperature and shall conform to the required values in tensile strength and elongation. Tubing shall meet several tests such as; pressure test, flattening test, and mechanical test.

Related Products

ASTM B183-79(1997)

ASTM B183-79(1997)

Standard Practice for Preparation of Low-Carbon Steel for Electroplating..

$23.00 $46.80

ASTM C1025-91(2000)

ASTM C1025-91(2000)

Standard Test Method for Modulus of Rupture in Bending of Electrode Graphite..

$23.00 $46.80

ASTM D5847-02

ASTM D5847-02

Standard Practice for Writing Quality Control Specifications for Standard Test Methods for Water Ana..

$30.00 $60.00

ASTM E140-05e1

ASTM E140-05e1

Standard Hardness Conversion Tables for Metals Relationship Among Brinell Hardness, Vickers Hardness..

$38.00 $76.80