• ASTM F1698-02
Provide PDF Format

Learn More

ASTM F1698-02

  • Standard Practice for Installation of Poly(Vinyl Chloride)(PVC) Profile Strip Liner and Cementitious Grout for Rehabilitation of Existing Man-Entry Sewers and Conduits
  • standard by ASTM International, 09/10/2002
  • Publisher: ASTM

$26.00$52.80


1.1 This practice describes the procedures for the rehabilitation of sewer lines and conduits by the installation of a field-fabricated PVC liner. After installation of the liner, cementitious grout is injected into the annular space between the liner and the existing sewer or conduit. The rehabilitation of the host structure by this installation practice results in a rigid composite structure (PVC/grout/existing pipe). This rehabilitation process may be used in a variety of gravity applications, such as sanitary sewers, storm sewers and process piping of man-entry sizes (36 to 144 in. in vertical dimension). The profile strips used for field fabrication of PVC liners are supplied in coils for spiral winding of the liner or in custom-cut flat panels for circumferential lining of all or any portion of the circumference of the host conduit (see Figs.1 and 2).

1.2 The values in parentheses are provided for information purposes only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Particular attention is drawn to those safety regulations and requirements involving entering into and working in confined spaces.

Related Products

ASTM B965-09(2014)

ASTM B965-09(2014)

Standard Specification for High Performance Tin-Coated Annealed Copper Wire Intended for Electrical..

$22.00 $44.00

ASTM D6172-98e1

ASTM D6172-98e1

Standard Test Method for Determining the Volume of Bulk Materials Using Contours or Cross Sections C..

$26.00 $52.80

ASTM D6386-16a

ASTM D6386-16a

Standard Practice for Preparation of Zinc (Hot-Dip Galvanized) Coated Iron and Steel Product and H..

$22.00 $44.00

ASTM C110-09a

ASTM C110-09a

Standard Test Methods for Physical Testing of Quicklime, Hydrated Lime, and Limestone..

$38.00 $76.80