  • Plating, Brush, Nickel Low Stress, Medium-Hardness Deposit
  • standard by SAE International, 04/01/2011
  • Publisher: SAE

$37.00$74.00


This specification covers the engineering requirements and process for brush plating of medium-hardness, low stress nickel by electrodeposition. It should be used, in conjunction with AMS 2451, for medium-hardness, low stress nickel deposits.

This process has been used typically to provide wear resistance and to repair damaged, worn, or mismachined parts in applications requiring hardness, fatigue resistance, and service temperatures up to 450 degrees F (232 degrees C), but usage is not limited to such applications.

Related Products

SAE ARP4737SUP1A

SAE ARP4737SUP1A

Aircraft Deicing/Anti-Icing Methods (Supplement 1) (Cancelled: Jan 2004)..

$37.00 $74.00

SAE AMS4191J

SAE AMS4191J

Aluminum Alloy, Welding Wire 6.3Cu - 0.30Mn - 0.18Zr - 0.15Ti - 0.10V (2319)..

$37.00 $74.00

SAE AS 3601

SAE AS 3601

Nut, Floating, Self-Locking, Attached Retention Element, 450\mDF, 125 ksi Ftu, UNS S66286 ( Reaffirm..

$37.00 $74.00

SAE AS4309D

SAE AS4309D

FITTING, NIPPLE, FLARED TUBE TO PIPE THREAD, FOR SEAL RING..

$37.00 $74.00