• SAE AMS2759/1E
Provide PDF Format

Learn More

SAE AMS2759/1E

  • Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)
  • standard by SAE International, 02/06/2009
  • Publisher: SAE

$37.00$74.00


This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS 2759.