  • Cobalt Alloy, Corrosion and Heat-Resistant, Strip 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated, Cold Rolled, and Aged Vacuum Induction Plus Vacuum Consumable Electrode Melted
  • standard by SAE International, 12/01/2012
  • Publisher: SAE

$37.00$74.00


This specification covers a corrosion and heat resistant cobalt alloy in the form of strip 0.100 inch (2.54 mm) and under in specified thickness and 4.000 inches (101.60 mm) and under in specified width. This strip has been used typically for springs requiring a combination of high strength up to 800 degrees F (425 degrees C), excellent corrosion resistance, and good fatigue properties, but usage is not limited to such applications. Alloy is nonmagnetic.

Related Products

SAE AMS4206A

SAE AMS4206A

Aluminum Alloy, Plate (7055-T7751) 8.0Zn 2.3Cu 2.0Mg 0.16Zr Solution Heat Treated, Stress Relieved, ..

$37.00 $74.00

SAE ARP4874A

SAE ARP4874A

Electronic Propulsion Control/Aircraft Interface Control Documents (Cancelled: Aug 2013)..

$37.00 $74.00

SAE AIR1129

SAE AIR1129

Aerospace Ground Equipment Criteria for a Propellant Transfer Unit (Cancelled: Jan 1999)..

$37.00 $74.00

SAE AMS3378A

SAE AMS3378A

Sealant, Silicone, Two-Part, General Purpose Room Temperature Vulcanizing Non-Fuel Resistant..

$37.00 $74.00