WHILE EVERY APPLICATION HAS VARIABLES, CUSHIONED ABRASIVES ARE USEFUL BECAUSE THEY REDUCE PREPLATE FINISHING COSTS, AND IN MANY CASES THEY IMPROVE THE QUALITY OF THE PLATED PART IN FEWER STEPS. THIS PAPER COVERS THE USE OF CUSHIONED ABRASIVES FOR PREPLATE MECHANICAL SURFACE CONDITIONING.