  • Prediction Of Ductile Fracture In Forward Extrusion With Spherical Dies
  • standard by Society of Manufacturing Engineers, 11/01/2000
  • Publisher: SME

$9.00$18.00


This paper describes a technique that can be used for the prevention of chevron cracks (or central burst defects) during the cold forward extrusion process with spherical dies. To characterize the behavior of the material and predict the formation of chevron cracks, it is necessary to determine the flow stress and critical damage value (CDV) of the billet material. The flow stress is obtained by homogeneous compression tests. Critical damage value (CDV) is determined from FEM simulations correlated with non-homogeneous compression tests and notched tensile tests. Two different materials are evaluated: SAE 1137 (hot rolled) and SAE 1524 (spheroidized).

Related Products

SME MS910322

SME MS910322

A Parallel Processing Architecture For Robotic Control..

$9.00 $18.00

SME ER98-317

SME ER98-317

Teaching Introductory Manufacturing Experimental Design Using Taguchi Methodology..

$9.00 $18.00

SME MR94-168

SME MR94-168

Development Toward A Perfect Spool/Bore Fit..

$9.00 $18.00

SME MS900268

SME MS900268

Optical Materials And Elements For Laser Material Processing..

$9.00 $18.00