• TAPPI T 569 om-14
Provide PDF Format

Learn More

TAPPI T 569 om-14

  • Internal bond strength (Scott type)
  • standard by Technical Association of the Pulp and Paper Industry, 2014
  • Publisher: TAPPI

$25.00$49.00


This method defines a test that measures the energy required to rapidly delaminate a sheet-type speciment. The "Z" directional rupture is initiated by the impact of a pendulum having both a controlled mass and a controlled velocity that exceeds 6000 times the velocity of tensile strength and other dead-weight testers. The geometry of the apparatus causes the tensile stress to be rotational in nature with negligible shear stress on the specimen.

The method is suitable for both single and multi-ply paper and paperboard, including coated sheets and those that are laminated with synthetic polymer films.

Related Products

TAPPI TIP 0410-05 (R2010)

TAPPI TIP 0410-05 (R2010)

Head of Stock Behind Slice (Head/Jet and Slice Flow Rate Relationships)..

$27.00 $53.00

TAPPI TIP 0416-14

TAPPI TIP 0416-14

Water Quality Guidelines and Monitoring Requirements for Paper Mill Boilers Operating with Softened ..

$25.00 $49.00

TAPPI TIP0304-44

TAPPI TIP0304-44

Using Washup Water as the Vehicle in Starch Based Corrugating Adhesive..

$25.00 $49.00

TAPPI TIP0302-03

TAPPI TIP0302-03

Corrugator Roll/Pressure Roll Journal Failures..

$25.00 $49.00