Provide PDF Format
TAPPI T 807 om-11
- Bursting Strength of Linerboard
- standard by Technical Association of the Pulp and Paper Industry, 06/01/2011
- Publisher: TAPPI
$25.00$49.00
Scope and summary
1.1 This method describes a procedure for measuring the bursting strength of linerboard using a disk shapeddiaphragm. Basis weights for this method should be 98 g/m2 (20#/MSF) and higher. The minimum burst should be 350kPa (51 psi). This method may also be used to test paperboard.
1.1.1 A specimen is clamped between two platens with circular openings in their centers. An expansiblediaphragm is distended through the lower platen by means of hydraulic pressure until the specimen ruptures. Themaximum hydraulic pressure when the specimen ruptures is recorded.
1.2 For the bursting strength of paper with basis weights below 98 g/m2, use TAPPI T 403 "Bursting Strengthof Paper." For corrugated combined board, see TAPPI T 810 "Bursting Strength of Corrugated Board."
1.1 This method describes a procedure for measuring the bursting strength of linerboard using a disk shapeddiaphragm. Basis weights for this method should be 98 g/m2 (20#/MSF) and higher. The minimum burst should be 350kPa (51 psi). This method may also be used to test paperboard.
1.1.1 A specimen is clamped between two platens with circular openings in their centers. An expansiblediaphragm is distended through the lower platen by means of hydraulic pressure until the specimen ruptures. Themaximum hydraulic pressure when the specimen ruptures is recorded.
1.2 For the bursting strength of paper with basis weights below 98 g/m2, use TAPPI T 403 "Bursting Strengthof Paper." For corrugated combined board, see TAPPI T 810 "Bursting Strength of Corrugated Board."